Gewalztes Stahlrohr
NPS ⅛ bis NPS 31/2
| NPS | DN mm | OD Zoll (mm) | SCH 5 | SCH 10 | SCH 30 | SCH 40/STD | SCH 80 | SCH 120 | SCH 160 | XXS |
|---|---|---|---|---|---|---|---|---|---|---|
| ⅛ | 6 | 0,405 in (10,29) | 0,035 in (0,889) | 0.049 in (1.245) |
0.057 in (1,448) |
0.068 in (1.727) |
0.095 in (2.413) |
--- | --- | --- |
| ¼ | 8 | 0.540 in (13.72) | 0,049 Zoll (1,245) | 0,065 in (1,651) | 0.073 in (1.854) |
0.088 in (2.235) |
0.119 in (3.023) |
--- | --- | --- |
| ⅜ | 10 | 0.675 in (17.15) | 0,049 Zoll (1,245) | 0,065 in (1,651) | 0.073 in (1.854) |
0.091 in (2.311) |
0.126 in (3.2) |
--- | --- | --- |
| ½ | 15 | 0.840 in (21.34) | 0,065 Zoll (1,651) | 0,083 in (2,108) | --- | 0.109 in (2.769) |
0.147 in (3.734) |
--- | --- | 0,294 in (7,468) |
| ¾ | 20 | 1,050 in (26,67) | 0.065 in (1.651) | 0.083 in (2.108) | --- | 0.113 in (2.870) |
0.154 in (3.912) |
--- | --- | 0,308 Zoll (7,823) |
| 1 | 25 | 1,315 Zoll (33,40) | 0,065 in (1,651) | 0.109 in (2.769) | --- | 0.133 in (3.378) |
0.179 in (4.547) |
--- | --- | 0,358 in (9,093) |
| 11/4 | 32 | 1.66 in (42.16) | 0.065 in (1.651) | 0.109 in (2.769) | 0.117 in (2.972) |
0,14 Zoll (3,556) | 0.191 in (4.851) |
--- | --- | 0,382 in (9,703) |
| 11/2 | 40 | 1.900 in (48.26) | 0,065 in (1,651) | 0.109 in (2.769) | 0.125 in (3.175) |
0.145 Zoll (3,683) |
0,20 in (5,08) | --- | --- | 0.4 in (10.16) |
| 2 | 50 | 2,375 in (60,33) | 0.065 in (1.651) | 0,109 in (2,769) | 0.125 in (3,175) |
0.154 in (3.912) |
0.218 Zoll (5,537) |
0,25 in (6,350) | --- | 0,436 in (11,074) |
| 21/2 | 65 | 2,875 in (73,02) | 0.083 in (2.108) | 0.12 in (3.048) | 0.188 in (4.775) | 0.203 in (5,156) |
0.276 Zoll (7,01) |
0,3 Zoll (7,62) | 0,344 in (8,738) | 0,552 in (14,021) |
| 3 | 80 | 3.500 in (88.9) | 0,083 in (2,108) | 0,12 Zoll (3,048) | 0,188 in (4,775) | 0.216 in (5.486) |
0.3 in (7.620) | 0,35 Zoll (8,89) | 0,438 in (11,125) | 0,6 Zoll (15,24) |
| 31/2 | 90 | 4,0 Zoll (101,6) | 0.083 in (2.108) | 0.12 in (3.048) | 0.188 in (4.775) | 0.226 in (5.740) |
0.318 in (8.077) |
--- | --- | 0,636 in (16,154) |
NPS 4 bis NPS 9
| NPS | DN mm | OD Zoll (mm) | SCH 5 | SCH 10 | SCH 20 | SCH 30 | SCH 40/STD | SCH 60 | SCH 80 | SCH 100 | SCH 120 | SCH 140 | SCH 160 |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| 4 | 100 | 4,5 Zoll (114,3) | 0,083 Zoll (2,108) | 0.120 in (3.048) | --- | 0,188 in (4,775) | 0,237 in (6,02) | 0,281 in (7,137) | 0,337 in (8,56) | --- | 0.437 in (11.1) | --- | 0,531 in (13,487) |
| 41/2 | 115 | 5,0 Zoll (127,0) | --- | --- | --- | --- | 0.247 in (6.274) | --- | 0.355 in (9.017) | --- | --- | --- | --- |
| 5 | 125 | 5,563 in (141,3) | 0,109 Zoll (2,769) | 0,134 in (3,404) | --- | --- | 0.258 in (6.553) | --- | 0,375 in (9,525) --- | --- | 0,5 Zoll (12,7) | --- | 0,625 Zoll (15,875) --- |
| 6 | 150 | 6,625 Zoll (168,27) | 0.109 in (2.769) | 0.134 in (3.404) | --- | --- | 0.28 in (7.112) | --- | 0.432 in (10.973) | --- | 0.562 in (14.275) | --- | 0,719 in (18,263) |
| 8 | 200 | 8,625 Zoll (219,08) | 0,109 in (2,769) | 0,148 in (3,759) | 0,25 in (6,35) | 0,277 in (7,036) | 0,322 in (8,179) | 0,406 in (10,312) | 0,5 Zoll (12,7) | 0,593 in (15,062) | 0,718 in (18,237) | 0,812 in (20,625) | 0,906 Zoll (23,012) |
NPS 10 bis NPS 24
| NPS | DN mm | OD Zoll (mm) | SCH 5s | SCH 5 | SCH 10s | SCH 10 | SCH 20 | SCH 30 |
|---|---|---|---|---|---|---|---|---|
| 10 | 250 | 10.75 in (273.05) | 0,134 Zoll (3,404) | 0,134 Zoll (3,404) | 0,165 Zoll (4,191) | 0,165 in (4,191) | 0,25 Zoll (6,35) | 0,307 in (7,798) |
| 12 | 300 | 12.75 in (323.85) | 0,156 Zoll (3,962) | 0.165 in (4.191) | 0,18 Zoll (4,572) | 0,18 Zoll (4,572) | 0,25 Zoll (6,35) | 0.33 in (8.382) |
| 14 | 350 | 14.0 in (355.6) | 0,156 Zoll (3,962) | 0,156 Zoll (3,962) | 0,188 in (4,775) | 0.250 in (6.350) | 0,312 Zoll (7,925) | 0,375 Zoll (9,525) |
| 16 | 400 | 16,0 Zoll (406,4) | 0.165 in (4.191) | 0.165 in (4.191) | 0,188 Zoll (4,775) | 7,925 Zoll (0,312 Zoll) | 0,25 Zoll (6,35) | 0,375 Zoll (9,525) |
| 18 | 450 | 18.00 in (457.20) | 0,165 Zoll (4,191) | 0,165 Zoll (4,191) | 0,188 Zoll (4,775) | 7,925 Zoll (0,312 Zoll) | 0,25 in (6,35) | 0,437 Zoll (11,1) |
| 20 | 500 | 20 Zoll (508) | 0,188 Zoll (4,775) | 0,188 Zoll (4,775) | 0,218 Zoll (5,537) | 0,375 in (9,525) | 0,25 Zoll (6,35) | 0,5 Zoll (12,7) |
| 24 | 600 | 24 Zoll (609,6) | 0,218 Zoll (5,537) | 0,25 Zoll (6,35) | 0,218 Zoll (5,537) | 0,25 Zoll (6,35) | 0,375 Zoll (9,525) | 0,562 Zoll (14,275) |
| NPS | SCH 40er | SCH 40 | SCH 60 | SCH 80er | SCH 80 | SCH 100 | >SCH 120 | SCH 140 | SCH 160 |
|---|---|---|---|---|---|---|---|---|---|
| 10 | 0,365 Zoll (9.271) | 0,365 Zoll (9,271) | 0,5 Zoll (12,7) | 0,5 Zoll (12,7) | 0,593 Zoll (15,062) | 0,718 Zoll (18,237) | 0.843 in (21.412) | 25,4 Zoll (1,0 Zoll) | 1,125 Zoll (28,575) |
| 12 | 0,375 Zoll (9,525) | 0.406 in (10.312) | 0,5 Zoll (12,7) | 0,5 Zoll (12,7) | 0,687 Zoll (17,45) | 0.843 in (21.412) | 25,4 Zoll (1,0 Zoll) | 1,125 Zoll (28,575) | 1,312 Zoll (33,325) |
| 14 | 0,375 Zoll (9,525) | 0,437 in (11,1) | 0,593 in (15,062) | 0.5 in (12.7) | 0,75 Zoll (19,05) | 0.937 in (23.8) | 1.093 in (27.762) | 1,25 Zoll (31,75) | 1.406 in (35.712) |
| 16 | 0,375 Zoll (9,525) | 0.5 in (12.7) | 0.656 in (16.662) | 0,5 Zoll (12,7) | 0.843 in (21.412) | 1,031 Zoll (26,187) | 1.218 in (30.937) | 1,437 in (36,5) | 1.593 in (40.462) |
| 18 | 0,375 Zoll (9,525) | 0,562 Zoll (14,275) | 0,750 Zoll (19,05) | 0,5 Zoll (12,7) | 0,937 in (23,8) | 1,156 Zoll (29,362) | 1.375 in (34.925) | 1,562 in (39,675) | 1,781 in (45,237) |
| 20 | 0,375 Zoll (9,525) | 0,593 Zoll (15,062) | 0.812 in (20.625) | 0,5 Zoll (12,7) | 1.031 in (26.187) | 1.280 in (32.512) | 38,1 Zoll (1,5 Zoll) | 1,75 Zoll (44,45) | 1,968 in (49,987) |
| 24 | 0,375 Zoll (9,525) | 0,687 in (17,45) | 0.968 in (24.587) | 0,5 Zoll (12,7) | 1.218 in (30.937) | 1.531 in (38.887) | 1.812 in (46.025) | 2,062 Zoll (52,375) | 2.343 in (59.512) |