12X18H10T-M |
EP2 |
1.4541 |
321 |
X12CrNiTi18-10 |
|
Edelstahl |
Band |
0,12х430mm |
GOST 4986-79, Авиатеxприемка |
38 |
Ru020 |
|
08X18H10 |
EI825 |
1.4301 |
304 |
X5CrNi1810 |
|
Edelstahl |
Band |
0,2h200 |
|
123 |
Ru010 |
|
ХН78Т |
EI435 |
2.4630 |
N06075 |
NiCr20Ti |
Nimonic 75® |
Nickel-Legierung |
Blatt |
1.5х650-710х1430 |
1-Blatt |
14kg |
Ru120 |
|
XN77TYUR |
EI437BU |
2.4952 |
N07080 |
NiCr20TiAl |
|
Nicrofer 7520Ti |
Blatt |
10,0х600х1430-1490 |
2лист-Blatt |
195kg |
Ru120 |
|
ХН38VT |
|
|
|
|
|
|
Blatt |
2,0х710х1380-1430 |
5лист-Blatt |
82kg |
Ru120 |
|
XH60VT |
EI868 |
|
|
|
|
Sonderlegierung |
Blatt |
0,5х270-430х1010-1420 |
Blatt-Blatt |
35kg |
Ru120 |
|
XH60VT |
EI868 |
|
|
|
|
Sonderlegierung |
Blatt |
0,8х720х1430 |
1-Blatt |
8kg |
Ru120 |
|
11X11N2V2MF-ш |
EI962 |
|
|
|
|
|
Blatt |
0.8х715х1430 |
1-Blatt |
6,5 kg |
Ru120 |
|
KhN56VMTYu |
EP199 |
|
|
|
|
Hitzebeständige Legierung |
Blatt |
1,0х710х1430 |
5лист-Blatt |
48kg |
Ru120 |
|
KhN68VMTYUK |
EP693 |
1.6932 |
|
28CrS4 |
|
Stahlbau |
Blatt |
2,0х715х1430 |
1L |
17kg |
Ru120 |
|
HN62VMYUT |
EP708 |
|
|
|
|
|
Blatt |
1,2х740-770х1430-1550 |
4лист-Blatt |
46kg |
Ru120 |
|
HN62VMYUT |
EP708 |
|
|
|
|
|
Blatt |
1,8х630-710х1270-1430 |
3лист-Blatt |
42kg |
Ru120 |
|
KhN45MVTYuBR-ид |
EP718 |
|
|
|
|
Hitzebeständige Legierung |
Blatt |
#1,5х530-705х1020-1430mm |
|
195 |
Ru130 |
|
XN50VMTYUB |
EP648 |
|
|
|
|
Hitzebeständige Legierung |
Blatt |
#0,8х715х1430mm |
|
220 |
Ru130 |
|
XN50VMTYUB |
EP648 |
|
|
|
|
Hitzebeständige Legierung |
Blatt |
#1х715х1430mm |
|
251 |
Ru130 |
|
XN50VMTYUB |
EP648 |
|
|
|
|
Hitzebeständige Legierung |
Blatt |
#2х715х1430mm |
|
17 |
Ru130 |
|
XN50MVKTYUR |
ЭП99 |
|
|
|
|
Hitzebeständige Legierung |
Blatt |
#0,8х720х1430mm |
|
230 |
Ru130 |
|
XN50MVKTYUR |
ЭП99 |
|
|
|
|
Hitzebeständige Legierung |
Blatt |
#2х720х1430mm |
|
90 |
Ru130 |
|
XH60VT |
EI868 |
|
|
|
|
Sonderlegierung |
Blatt |
#1,8х1000х1430mm |
|
203 |
Ru130 |
|
XH60VT |
EI868 |
|
|
|
|
Sonderlegierung |
Blatt |
#1,8х715х1430mm |
|
17 |
Ru130 |
|
XH60VT |
EI868 |
|
|
|
|
Sonderlegierung |
Blatt |
#2,5х715х1430mm |
|
24 |
Ru130 |
|
ХН78Т |
EI435 |
2.4630 |
N06075 |
NiCr20Ti |
Nimonic 75® |
Nickel-Legierung |
Blatt |
#1,4х715х1430mm |
|
38 |
Ru130 |
|
07X16H6 |
ЭИ288 |
|
301 |
X12CrNi17-7 |
|
Edelstahl |
Blatt |
2,0 x 710 x 1430 mm |
|
70 kg |
Ru150 |
|
12Х21Н5Т |
EI811 |
|
|
|
|
Edelstahl |
Blatt |
4,0 x 1000 x 2430 mm |
|
148 kg |
Ru150 |
|
12Х21Н5Т |
EI811 |
|
|
|
|
Edelstahl |
Blatt |
6,0 x 500-970х2400-4430 mm |
|
224 kg |
Ru150 |
|
12Х21Н5Т |
EI811 |
|
|
|
|
Edelstahl |
Blatt |
20,0х430-1170х1310-1580 mm |
|
816 kg |
Ru150 |
|
04Х18Н10 |
EI842 |
1.4307 |
304L |
X2CrNi18-9 |
|
Edelstahl |
Draht |
2,0 mm |
|
20 kg |
Ru150 |
|
17X18H9 |
EYA1 |
1.4300 |
301 |
X10CrNiTi18-9 |
|
Edelstahl |
Draht |
0,3 mm |
|
67 kg |
Ru150 |
|
17X18H9 |
EYA1 |
1.4300 |
301 |
X10CrNiTi18-9 |
|
Edelstahl |
Draht |
0,4 mm |
|
24 kg |
Ru150 |
|
08.17 |
~~ EI645 |
1.4510 |
430Ti |
X6CrTi17 |
|
Edelstahl |
Quadrat |
50х50х3155 mm |
|
56 kg |
Ru150 |
|
17X18H9 |
EYA1 |
1.4300 |
301 |
X10CrNiTi18-9 |
|
Edelstahl |
Kreis |
1,0 mm |
Silberfischchen |
49 kg |
Ru150 |
|
08X18H10 |
EI825 |
1.4301 |
304 |
X5CrNi1810 |
|
Edelstahl |
Band |
0,3х400 |
|
1000 |
Ru210 |
|
08X18H10 |
EI825 |
1.4301 |
304 |
X5CrNi1810 |
|
Edelstahl |
Band |
0,65х410 |
|
530 |
Ru210 |
|
08X18H10 |
EI825 |
1.4301 |
304 |
X5CrNi1810 |
|
Edelstahl |
Blatt |
1.5 |
4L |
36 |
Ru210 |
|
08X18H10 |
EI825 |
1.4301 |
304 |
X5CrNi1810 |
|
Edelstahl |
Blatt |
2 |
|
49 |
Ru210 |
|
08X18H10 |
EI825 |
1.4301 |
304 |
X5CrNi1810 |
|
Edelstahl |
Blatt |
2 |
|
55 |
Ru210 |
|
08X18H10 |
EI825 |
1.4301 |
304 |
X5CrNi1810 |
|
Edelstahl |
Blatt |
2 |
|
55 |
Ru210 |
|
08X18H10 |
EI825 |
1.4301 |
304 |
X5CrNi1810 |
|
Edelstahl |
Blatt |
2 |
|
172 |
Ru210 |
|
08X18H10 |
EI825 |
1.4301 |
304 |
X5CrNi1810 |
|
Edelstahl |
Blatt |
4 |
|
128 |
Ru210 |
|
08X18H10 |
EI825 |
1.4301 |
304 |
X5CrNi1810 |
|
Edelstahl |
Blatt |
5 |
|
160 |
Ru210 |
|
VT1-0 |
|
3.7035 |
R50400 |
|
Titan Grade 2 |
Titanmetall |
Rohr |
22х2х4000-4300mm |
|
226 |
Ru240 |
|
VT1-0 |
|
3.7035 |
R50400 |
|
Titan Grade 2 |
Titanmetall |
Rohr |
25х2х300-1000-4300-5000 mm |
|
179.5 |
Ru240 |
|
PT7M |
|
|
|
|
|
|
Rohr |
325х16х |
L = 4300мм 1 Stck. |
310 |
Ru240 |
|
PT1M |
|
|
|
|
|
|
Rohr |
45х2х3700-4300mm |
|
89.2 |
Ru240 |
|
BT5 |
|
3.7115 |
R54520 |
Ti5Al2.5Sn |
Titan Grade 6 |
Titanmetall |
Kreis |
20х1430 |
VFR |
2 |
Ru250 |
|
BT8 |
|
|
|
|
Titanium Gost VT8 |
Titanmetall |
Kreis |
60х3430 |
G/K |
30,6 |
Ru250 |
|
VT1-0 |
|
3.7035 |
R50400 |
|
Titan Grade 2 |
Titanmetall |
Blatt |
3х430х1030 |
|
21,2 |
Ru250 |
|
VT1-0 |
|
3.7035 |
R50400 |
|
Titan Grade 2 |
Titanmetall |
Blatt |
8х1000х1430 |
|
52,8 |
Ru250 |
|
VT1-0 |
|
3.7035 |
R50400 |
|
Titan Grade 2 |
Titanmetall |
Blatt |
12х430х1220 |
|
28,7 |
Ru250 |
|
VT1-0 |
|
3.7035 |
R50400 |
|
Titan Grade 2 |
Titanmetall |
Blatt |
40х130х430 |
|
11,1 |
Ru250 |
|
BT6 |
|
3.7165 |
R56200 |
6AL4V |
Titan Grade 5 |
Titanmetall |
Blatt |
8х430х980 |
ВТ6с |
15,5 |
Ru250 |
|
VA |
EEP |
|
WP |
EWP |
Wolfram 99,95% |
Grüne Elektrode |
Elektrode |
ø10х430-630 mm |
|
2,4 kg |
Ru310 |
|
св I-1 |
EVI-1 |
|
|
|
|
Wolframelektrode |
Elektrode |
ø8х~430 mm |
|
3,4 kg |
Ru310 |
|
св I-1 |
EVI-1 |
|
|
|
|
Wolframelektrode |
Elektrode |
ø17х430 |
|
1,75 kg |
Ru310 |
|
MCH |
|
|
|
|
Molybdenum 99,96% |
Molybdän-Metall |
Kreis |
ø6х430х700 mm |
|
4 kg |
Ru310 |
|
MCH |
|
|
|
|
Molybdenum 99,96% |
Molybdän-Metall |
Kreis |
ø14х430-720 mm |
|
4,7 kg |
Ru310 |
|
MCH |
|
|
|
|
Molybdenum 99,96% |
Molybdän-Metall |
Kreis |
ф50х1430 mm |
|
29 kg |
Ru310 |
|
MCH-1 |
|
|
|
|
|
|
Rohr |
ø14х1х430-650 mm |
|
0,64 kg |
Ru310 |
|
MCH-1 |
|
|
|
|
|
|
Rohr |
ø20х2х360-430 mm |
|
1,5 kg |
Ru310 |
|
MCH-1 |
|
|
|
|
|
|
Rohr |
ø22х2х430 mm |
|
2,4 kg |
Ru310 |
|
MCH-1 |
|
|
|
|
|
|
Rohr |
ø30х2х330-430 mm |
|
5,1 kg |
Ru310 |
|
MCH-1 |
|
|
|
|
|
|
Rohr |
ø30х2х430 mm |
|
5,55 kg |
Ru310 |
|
NBC-1 |
|
|
|
|
|
Nioblegierung |
Rohr |
ø27х2,5 L 200-430 mm |
|
2, kg |
Ru310 |
|
5VIC |
|
|
|
|
|
|
Kreis |
ø55х420х430 mm |
|
35,9 kg |
Ru310 |
|
Х18Н10 |
EYA1 |
1.4300 |
301 |
X10CrNi18-10 |
|
Edelstahl |
Blatt |
6 x 675 x 1377 mm mm |
|
45,6 kg |
Ru310 |
|
|
VZH101 |
|
|
|
|
|
Blatt |
2х715х1430 mm |
|
16,5 kg |
Ru310 |
|
|
VZH101 |
|
|
|
|
|
Blatt |
2х715х1430 mm |
|
16 kg |
Ru310 |
|
|
VZH101 |
|
|
|
|
|
Blatt |
2х710х1430 mm |
|
17 kg |
Ru310 |
|
|
VZH101 |
|
|
|
|
|
Blatt |
2х715х1430 mm |
|
16 kg |
Ru310 |
|
36НХТЮ |
EI702 |
1.3918 |
N09902 |
|
Elinvar® |
Ni-SpanC902 |
Blatt |
1*720*1430mm |
|
8.3 |
Ua010 |
Ukraine |
08X17 |
~~ EI645 |
1.4016 |
430 |
X6Cr17 |
|
Edelstahl |
Band |
0,25х200 |
|
19.7 |
Ua010 |
Ukraine |
08X17 |
~~ EI645 |
1.4016 |
430 |
X6Cr17 |
|
Edelstahl |
Band |
0,2х400 |
|
668.45 |
Ua010 |
Ukraine |
08X17 |
~~ EI645 |
1.4016 |
430 |
X6Cr17 |
|
Edelstahl |
Band |
0,25х400 |
|
207.15 |
Ua010 |
Ukraine |
08X17 |
~~ EI645 |
1.4016 |
430 |
X6Cr17 |
|
Edelstahl |
Band |
0,3х400 |
|
562.85 |
Ua010 |
Ukraine |
08X17 |
~~ EI645 |
1.4016 |
430 |
X6Cr17 |
|
Edelstahl |
Band |
0,35х400 |
|
522.2 |
Ua010 |
Ukraine |
08X17 |
~~ EI645 |
1.4016 |
430 |
X6Cr17 |
|
Edelstahl |
Band |
0,4х400 |
|
317.45 |
Ua010 |
Ukraine |
08X17 |
~~ EI645 |
1.4016 |
430 |
X6Cr17 |
|
Edelstahl |
Band |
0,5х400 |
|
472.15 |
Ua010 |
Ukraine |
08X18H10 |
EI825 |
1.4301 |
304 |
X5CrNi1810 |
|
Edelstahl |
Blatt |
0,9х1000х2000 |
1Stück |
1 |
Ua010 |
Ukraine |
08.17 |
~~ EI645 |
1.4510 |
430Ti |
X6CrTi17 |
|
Edelstahl |
Draht |
F3,0mm |
|
89.6 |
Ua010 |
Ukraine |
08X18H10 |
EI825 |
1.4301 |
304 |
X5CrNi1810 |
|
Edelstahl |
Rohr |
42,4х2mm |
6метр |
1 |
Ua010 |
Ukraine |
08X18H10 |
EI825 |
1.4301 |
304 |
X5CrNi1810 |
|
Edelstahl |
Rohr |
6x1,4mm 2030mm |
|
1 |
Ua010 |
Ukraine |
08X18H10 |
EI825 |
1.4301 |
304 |
X5CrNi1810 |
|
Edelstahl |
Band |
0.3х400 |
Weiche |
19.2 |
Ua120 |
Ukraine |
08X18H10 |
EI825 |
1.4301 |
304 |
X5CrNi1810 |
|
Edelstahl |
Band |
0.6х400 |
Weiche |
11.2 |
Ua120 |
Ukraine |
HN75MBTYu |
EI602 |
2.4856 |
N06625 |
NiCr22Mo9Nb |
Inconel 625® |
Nickel-Legierung |
Kreis |
Ф38 Abmessungen in mm = 680 850 430 700 610 590 270 280 470 770 260 800 360 840 760 690 660 350 370 760 700 710 640 390 370 290 590 440 340 |
|
|
Ua120 |
Ukraine |
HN75MBTYu |
EI602 |
2.4856 |
N06625 |
NiCr22Mo9Nb |
Inconel 625® |
Nickel-Legierung |
Kreis |
Ф120 mm Abmessungen = 150 150 430 |
|
20 |
Ua120 |
Ukraine |
08X18H10 |
EI825 |
1.4301 |
304 |
X5CrNi1810 |
|
Edelstahl |
Draht |
Durchmesser 1,2 |
|
13.6 |
Ua140 |
Ukraine |
08X18H10 |
EI825 |
1.4301 |
304 |
X5CrNi1810 |
|
Edelstahl |
Draht |
Durchmesser 2,0 |
|
21.8 |
Ua140 |
Ukraine |
08X18H10 |
EI825 |
1.4301 |
304 |
X5CrNi1810 |
|
Edelstahl |
Draht |
Durchmesser 2,5 |
|
71.2 |
Ua140 |
Ukraine |
08X18H10 |
EI825 |
1.4301 |
304 |
X5CrNi1810 |
|
Edelstahl |
Draht |
Durchmesser 3,0 |
|
205 |
Ua140 |
Ukraine |
08X18H10 |
EI825 |
1.4301 |
304 |
X5CrNi1810 |
|
Edelstahl |
Draht |
Durchmesser 4,0 |
|
5.4 |
Ua140 |
Ukraine |
08X18H10 |
EI825 |
1.4301 |
304 |
X5CrNi1810 |
|
Edelstahl |
Draht |
Durchmesser 6,0 |
|
73 |
Ua140 |
Ukraine |
12X18H10T |
EP2 |
1.4541 |
321 |
X12CrNiTi18-10 |
|
Edelstahl |
Rohr |
Ø33x1,5 |
(L=1770-4300) GOST 9941-81 |
610 |
Ua150 |
Ukraine |
08X18H10 |
EI825 |
1.4301 |
304 |
X5CrNi1810 |
|
Edelstahl |
Rohr |
6 x 1,0 |
6M(25,1 kg) |
25.1 |
Ua210 |
Ukraine |
08X18H10 |
EI825 |
1.4301 |
304 |
X5CrNi1810 |
|
Edelstahl |
Rohr |
6 x 2,0 |
6M(24,4 kg) |
24.4 |
Ua210 |
Ukraine |
08X18H10 |
EI825 |
1.4301 |
304 |
X5CrNi1810 |
|
Edelstahl |
Rohr |
8 x 1,0 |
4,8-6,3 m(152,8 kg) |
152.8 |
Ua210 |
Ukraine |
08X18H10 |
EI825 |
1.4301 |
304 |
X5CrNi1810 |
|
Edelstahl |
Rohr |
10 x 3,0 |
6,75 m; 1,6 m(0,8 kg) - 1Stück |
5.2 |
Ua210 |
Ukraine |
08X18H10 |
EI825 |
1.4301 |
304 |
X5CrNi1810 |
|
Edelstahl |
Rohr |
14 x 1,0 |
3-6M(74,7 kg) geschweißte |
74.7 |
Ua210 |
Ukraine |
08X18H10 |
EI825 |
1.4301 |
304 |
X5CrNi1810 |
|
Edelstahl |
Rohr |
14 x 3,0 |
6M(32kg) |
32.0 |
Ua210 |
Ukraine |
08X18H10 |
EI825 |
1.4301 |
304 |
X5CrNi1810 |
|
Edelstahl |
Rohr |
16 x 3,0 |
5-6,4 m(335kg); 3,4-4,5 m(97kg) |
432.0 |
Ua210 |
Ukraine |
08X18H10 |
EI825 |
1.4301 |
304 |
X5CrNi1810 |
|
Edelstahl |
Rohr |
25 x 1,0 |
3,1 m(1,8 kg) - geschweißte 1Stück |
1.8 |
Ua210 |
Ukraine |