Die Preisliste
Lager
Zusätzliche Felder
Markierung | W. Nr. | Titel | Stahl Typ | Form | Größe | Kommentar | Die Balance |
---|---|---|---|---|---|---|---|
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 0.5х600х1600-2000 | 2St | 4.4 |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 0.8х500-510х770-1200 | Karten | 28.4 |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 1х400х1380 | Karten | 5 |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 1.5х370-770х450-1420 | Karten | 22.4 |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 2х1000х2000 VSMPO | маркир | 92.5 |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 2х270-530х500-1100 | Karten | 15.6 |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 3х1000х2000 VSMPO | маркир | 108 |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 3х300-1060х440-2000 | Karten | 129 |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 4х270-700х400-1860 | Karten | 268 |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 4х1000х2000 | VSMPO, mit Reserve | 39 |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 5х300-890х500-1000 | Karten | 155 |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 6х650-1000х1200-2000 | GOST 22178-76 | 841 |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 6х500х800 | Karten | 10.6 |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 8х200-350х255-1000 | Karten | 31 |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 10х240-290х260-355 | Karten | 10.2 |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 12х1000х2000 | 430 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 16х170х800 | Karten | 10 |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 36х1500х1500 | 729 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 36х460х2465 | 182 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 50х320х2319 | 168 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 50х673х1492 | 227 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 0.3х600х1500 | 5er | 6,1 |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 0.4х600х2000 | 4St | 9,2 |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 0.5х600х2000 | 32,1 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 0.6х600х2000 | 116,6 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 0.6х600х1500 | 2,2 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 0.8х1000х2000 | 2St 7,3 kg + 7,3 kg | 14,6 |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 0.8х800х2000 | 11шт | 66,4 |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 0.8х1000х2000 | 5er | 40,4 |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 0.8х600х2000 | 50,3 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 0.8х600х1500 | 1Stück | 3,3 |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 0.8х1000х2000 | 5er | 37,9 |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 0.8х500х2000 | 2St | 7,9 |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 1х1000х2000 | 104,5 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 1х1000х2000 | 47,3 (9,5x3шт+9,4x2шт) | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 1х370-380х600 | 64,6 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 1х1000х2000 | 4St | 38,2 |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 1х1000х2000 | 2 Stück 9,5 kg + 9,5 kg | 19 |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 1.2х1000х2000 | 4St | 44 |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 1.2х800х2000 | 7шт | 63,2 |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 1.2х600х2000 | 2St | 13,2 |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 2х1000х1480 | Stempel | 13,6 |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 2х750х1000 | 6,7 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 2х1000х1000 | 4St | 35 |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 2х800х1840 | 13,5 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 3х625х695 | 5,9 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 3х1000х1250 | 17,4 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 3х860х1000 | 12,2 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 3х430х1030 | 21,2 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 3х910х1320 | 16,7 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 3х800х2000 | 2St | 42,9 |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 3х930х1360 | 17,4 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 3х800х2000 | 2St (21,5 kg+21,4 kg) | 42.9 |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 4х600х1000 | 42,9 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 4х735х1100 | 13,1 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 4х580х760 | 8,2 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 4х760х1000 | 13,9 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 4х1005х1520 | 2St | 54,9 |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 4х540х1955 | 19 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 4х745х990 | 13,2 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 4х600х920 | 9,9 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 4х740х1000 | 13,6 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 4х765х920 | 13,1 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 4х600х800 | 8,5 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 4х600х1500 | 16,5 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 4х570х900 | 9,3 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 4х1000х2000 | 36,3 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 5х1000х2000 | 49,7 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 5х600х2000 | 27,6 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 5х660х820 | 12,4 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 5х600х2000 | 27,6 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 6х500х680 | 9,6 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 6х1000х1500 | 42,6 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 8х1000х1430 | 52,8 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 8х1000х2000 | 74,7 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 10х470х630 | 13,5 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 10х230х350 | 3,8 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 10х520х830 | 19,7 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 10х1000х1455 | 67 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 10х490х630 | 14 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 10х190х260 | 2,4 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 10х480х850 | 19,2 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 10х500х630 | 14,4 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 10х160х310 | 2,4 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 10х290х520 | 7 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 10х1000х2000 | 1Stück | 90,5 |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 10х505х695 | 14,5 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 10х120х520 | 3,2 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 10х285х340 | 3,4 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 10х800-910 | 33,1 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 10х930х990 | 42,2 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 10х100х560 | 2,7 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 10х250х480 | 5,5 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 10х800х1010 | 36,8 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 10х910х940 | 38,6 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 10х240х1000 | 10,6 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 10х870х930 | 37,6 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 12х570х1100 | 33 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 12х470х500 | 13,6 | |
VT1-0 | 3.7035 | Titan Grade 2 | Titanmetall | Blatt | 12х430х1220 | 28,7 |