Die Preisliste
Lager
Zusätzliche Felder
Markierung | W. Nr. | Titel | Stahl Typ | Form | Größe | Kommentar | Die Balance |
---|---|---|---|---|---|---|---|
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 15х1100-1740 | G/K | 54.5 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 80х580 | G/K | 13.5 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 5х1000х1060 | 23 | ||
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 10 | 38,3 | ||
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 14х520-1030 | G/K | 16,1 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 16х2170 | G/K | 4,7 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 18х2740 | shlif. | 3,1 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 18х1730-2370 | VFR | 4,9 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 20х1010-1110 | shlif. | 4,5 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 20х500-2500 | m/O | 17,8 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 25х800-1300 | shlif. | 39 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 27х1000 | 2,8 | ||
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 28х1055-1120 | 3kg+2,9 kg | 5,9 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 30х1080-1120 | Kaliber. | 13,9 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 30х480-1450 | G/K | 25,1 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 30х1130 | shlif. | 3,5 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 32х1110 | shlif. | 4 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 35х900-1130 | shlif. | 65,3 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 35х1060-1120 | shlif. | 28,5 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 38х1085-1145 | 4St Kaliber. | 22,6 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 38х1120 | shlif. | 5,7 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 40х300-365 | 22шт Kaliber. | 39,7 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 40х1095-1130 | shlif. | 31,4 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 40х1090-2810 | shlif. | 223,4 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 40х690 | Kaliber. | 3,9 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 45х1080 | Kaliber. | 7,7 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 45х680 | Kaliber. | 4,9 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 50х450 | G/K | 4 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 50х1070-1150 | 10kg+9,4 kg Kern. | 19,4 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 50х1060-1130 | 2St Kaliber. | 19,2 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 55х1055-1115 | 4St Kaliber. | 45,7 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 55х1145 | shlif. | 12,3 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 55х420 | Kaliber. | 4,4 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 60х445-1050 | G/K | 80,5 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 65х1045-1110 | 3tlg Kaliber. | 48,1 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 70х1030-1100 | 2St Kaliber. | 37,2 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 70х595-1970 | G/K | 64,3 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 75х1000 | G/K | 20,3 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 80х1035-1125 | 2St Kaliber. | 49,8 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 80х370 | shlif. | 8 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 90х570 | G/K VFR VSMPO | 16,6 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 90 | 28 | ||
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 100х1425 | shlif. | 51 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 100х1060 | shlif. | 37,9 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 100х1005-1060 | 2St Kaliber. | 73,8 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 120х1095 | Kaliber. | 56,2 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 130х340 | G/K | 20,9 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 130х450 | m/O | 26,8 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 130х570 | m/O | 35,1 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 130х630 | m/O | 38,7 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 150х360 | m/O | 28,9 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 200х480 | m/O | 66,9 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 240х340 | Ing. | 72 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 240х40 | 8,3 | ||
BT20 | Titanium Gost VT20 | Titanmetall | Blatt | 0.8х600х2000 | 9,3 | ||
BT20 | Titanium Gost VT20 | Titanmetall | Blatt | 1х600х1500 | 19,6 | ||
BT20 | Titanium Gost VT20 | Titanmetall | Blatt | 1х600х1500 | 41,9 | ||
BT20 | Titanium Gost VT20 | Titanmetall | Blatt | 1х600х2000 | 33,8 | ||
BT20 | Titanium Gost VT20 | Titanmetall | Blatt | 1.2х600х2000 | 1Stück | 6,6 | |
BT20 | Titanium Gost VT20 | Titanmetall | Blatt | 1.2х600х1500 | 24,6 | ||
BT20 | Titanium Gost VT20 | Titanmetall | Blatt | 1.2х600х1500 | 28,7 | ||
BT20 | Titanium Gost VT20 | Titanmetall | Blatt | 1.5х600х1500 | 149,2 | ||
BT20 | Titanium Gost VT20 | Titanmetall | Blatt | 1.8х600х2000 | 216,1 | ||
BT20 | Titanium Gost VT20 | Titanmetall | Blatt | 1.8х800х2000 | 159,8 | ||
BT20 | Titanium Gost VT20 | Titanmetall | Blatt | 2х800х1500 | 163,4 | ||
BT20 | Titanium Gost VT20 | Titanmetall | Blatt | 2х800х1500 | 207,5 | ||
BT20 | Titanium Gost VT20 | Titanmetall | Blatt | 2х1000х2000 | 5er | 92,5 | |
BT20 | Titanium Gost VT20 | Titanmetall | Blatt | 2х600х1500 | 15,4 | ||
BT20 | Titanium Gost VT20 | Titanmetall | Blatt | 2.5х800х2000 | 17,6 | ||
BT20 | Titanium Gost VT20 | Titanmetall | Blatt | 3х500-600х750 | 3tlg | 16,3 | |
BT20 | Titanium Gost VT20 | Titanmetall | Blatt | 3х750х810 | 1Stück | 8,4 | |
BT20 | Titanium Gost VT20 | Titanmetall | Blatt | 6х715х800 | 1Stück | 15,5 | |
BT20 | Titanium Gost VT20 | Titanmetall | Blatt | 6х800х1500 | 2St | 65 | |
BT20 | Titanium Gost VT20 | Titanmetall | Blatt | 6х500х1000 | 171,5 | ||
BT20 | Titanium Gost VT20 | Titanmetall | Blatt | 8х565х950 | 18,8 | ||
BT20 | Titanium Gost VT20 | Titanmetall | Blatt | 8х540х1120 | 22,1 | ||
BT20 | Titanium Gost VT20 | Titanmetall | Blatt | 8х515х920 | 16,8 | ||
BT20 | Titanium Gost VT20 | Titanmetall | Blatt | 8х510х930 | 17,2 | ||
BT20 | Titanium Gost VT20 | Titanmetall | Blatt | 8х570х1890 | 38,2 | ||
BT20 | Titanium Gost VT20 | Titanmetall | Blatt | 8х560х920 | 18,3 | ||
BT20 | Titanium Gost VT20 | Titanmetall | Blatt | 8х550х930 | 18,3 | ||
BT20 | Titanium Gost VT20 | Titanmetall | Blatt | 8х580х1000 | 20,9 | ||
BT20 | Titanium Gost VT20 | Titanmetall | Blatt | 9х600х600 | 16,1 | ||
BT20 | Titanium Gost VT20 | Titanmetall | Blatt | 9х605х670 | 1 Stück | 16,1 | |
BT20 | Titanium Gost VT20 | Titanmetall | Blatt | 10х500х1180 | 29,1 | ||
BT20 | Titanium Gost VT20 | Titanmetall | Blatt | 16х415х1030 | 31,1 | ||
BT20 | Titanium Gost VT20 | Titanmetall | Blatt | 16х570х1250 | 41,9 | ||
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 42хм.über die Länge und 2000mm | 300 | ||
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 44хм.über die Länge und 2000mm | 1000 | ||
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 45хм.über und 2000mm | 1600 | ||
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 55хм.über und 2000mm | 500 | ||
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 55 | 1500kg | ||
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 65хм.über und 2000mm | 400 | ||
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 120х | 1Stück m/O VSMPO | 46.5 | |
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 180 | 4000kg | ||
BT20 | Titanium Gost VT20 | Titanmetall | Kreis | 190 | 4500kg | ||
BT20 | Titanium Gost VT20 | Titanmetall | Blatt | 6.4x1000x2000 | 3tlg | unter die Bestellung | |
BT20 | Titanium Gost VT20 | Titanmetall | Blatt | 12 | 893kg | ||
BT20 | Titanium Gost VT20 | Titanmetall | Blatt | 14х500кг | unter die Bestellung | ||
BT20 | Titanium Gost VT20 | Titanmetall | Blatt | 40х1000х2500 | 2 Stück |